Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced N3U41G6 - PA9T-GF30 FR(40) - BASF

Material Data Center offers the following functions for Ultramid® Advanced N3U41G6:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Polyphthalamide, light colorable, with a high melting point, halogen-free flame-retardant, very low water absorption, good mechanical and dielectrical properties at elevated temperatures as well as excellent chemical resistance, soldering bath resistant. Colors available (e.g. Orange RAL 2003).

Markets & applications
Automotive: Automotive electrics & electronics (E&E), sensors, fuel cell, e-mobility
E&E: Connectors, SMT (surface mount technology) applications, energy distribution
Consumer goods: Home appliances, consumer electronics, cell phone parts
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 30 / * cm³/10min ISO 1133
Temperature 325 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.3 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 10500 / 10500 MPa ISO 527
Stress at break 140 / 130 MPa ISO 527
Strain at break 2.2 / 2.2 % ISO 527
Charpy impact strength, +23°C 60 / 50 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 60 / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6.5 / 6.5 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 300 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 265 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 19 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 53 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-0 / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Yellow Card available yes / * - -
Burning Behav. at thickness h V-0 / * class IEC 60695-11-10
Thickness tested 0.2 / * mm -
Yellow Card available yes / * - -
Burning Behav. 5V at thickness h 5VA / * class IEC 60695-11-20
Thickness tested 1.6 / * mm -
Yellow Card available yes / * - -
Oxygen index 38 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 1MHz 4.1 / 3.5 - IEC 62631-2-1
Dissipation factor, 1MHz 110 / 160 E-4 IEC 62631-2-1
Volume resistivity 1E13 / 1E13 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E15 Ohm IEC 62631-3-2
Electric strength 45 / 44 kV/mm IEC 60243-1
Comparative tracking index - / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 2.1 / * % Sim. to ISO 62
Humidity absorption 0.85 / * % Sim. to ISO 62
Density 1440 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 100 / * cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 330 °C ISO 294
Injection Molding, mold temperature 140 °C ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 8 h -
Processing humidity ≤0.05 % -
Melt temperature 310 - 340 °C -
Mold temperature 100 - 160 °C -
Diagrams
Viscosity-shear rate , Ultramid® Advanced N3U41G6, PA9T-GF30 FR(40), BASF
Shearstress-shear rate , Ultramid® Advanced N3U41G6, PA9T-GF30 FR(40), BASF
Stress-strain , Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Stress-strain , Ultramid® Advanced N3U41G6 (cond.), PA9T-GF30 FR(40), BASF
Secant modulus-strain , Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Secant modulus-strain , Ultramid® Advanced N3U41G6 (cond.), PA9T-GF30 FR(40), BASF
Stress-strain (isochronous) 23°C, Ultramid® Advanced N3U41G6 (cond.), PA9T-GF30 FR(40), BASF
Creep modulus-time 23°C, Ultramid® Advanced N3U41G6 (cond.), PA9T-GF30 FR(40), BASF
Creep curve 23°C, Ultramid® Advanced N3U41G6 (cond.), PA9T-GF30 FR(40), BASF
Stress-strain (isochronous) 60°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Creep modulus-time 60°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Creep curve 60°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Stress-strain (isochronous) 90°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Creep modulus-time 90°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Creep curve 90°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Stress-strain (isochronous) 120°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Creep modulus-time 120°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Creep curve 120°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Stress-strain (isochronous) 150°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Creep modulus-time 150°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Creep curve 150°C, Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Tensile modulus-temperature , Ultramid® Advanced N3U41G6 (dry), PA9T-GF30 FR(40), BASF
Tensile modulus-temperature , Ultramid® Advanced N3U41G6 (cond.), PA9T-GF30 FR(40), BASF
Characteristics
Processing
Injection Molding
Special Characteristics
Flame retardant, Halogen-free
Features
Melt Strength, Thermal Stability
Chemical Resistance
General Chemical Resistance
Applications
Automotive, Electrical and Electronical
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .05 %
Pre/Post-processing, Pre-drying, Temperature: 120 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 310 - 340 °C
injection molding, Melt temperature, recommended: 330 °C
injection molding, Mold temperature, range: 100 - 160 °C
injection molding, Mold temperature, recommended: 140 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.